← BlogCare & troubleshooting

Calcium Dissolution in Ceramic and Mosaic Grout Joints: Erosion of Cement-Based Grouts in Soft Water

Water with low calcium hardness tends to dissolve the free calcium in cement-based grout joints in order to reach its chemical balance, and over time this can lead to grout loss. Because PVC-based liner membranes have a synthetic polymer structure containing no calcium binder, they do not erode through this dissolution mechanism. The rate of erosion depends on the measured values of the water and on maintenance discipline.

7 min
Calcium Dissolution in Ceramic and Mosaic Grout Joints: Erosion of Cement-Based Grouts in Soft Water
Sermed Havuz photo · illustrative
Sermed Havuz technical team

Pool models, construction conditions and care to help you plan your project.

In this guide 4
  1. 01The Effect of Low Calcium Hardness and Unbalanced Water on Cement Grout Joints
  2. 02Langelier Saturation Index (LSI) Balance and the Chemical Behaviour of Liner Coverings
  3. 03Water Chemistry Comparison Table: Pool with Cement Grout Joints versus Liner-Covered Pool
  4. 04Frequently Asked Questions

Application note: Chemical dosages, pH/chlorine targets, operating times and maintenance intervals are determined according to the product label, the measured water values, the usage class and local requirements. Numerical examples on their own are not application instructions. Chemicals must never be mixed with one another; electrical work, pressurized equipment and pool draining operations must be carried out under expert supervision. The regional water values given in this article are not verified measurements but hypothetical planning examples used to illustrate the calculation logic; actual values are determined through laboratory or on-site analysis of the pool water.

Mains water fed from mountainous, high-rainfall catchments can generally be poorer in minerals and may turn out to have low calcium hardness, in other words a "soft water" character. In pool chemistry, water that is not saturated tends to dissolve the mineral it lacks out of the surfaces it comes into contact with. Water with a negative Langelier Saturation Index (LSI), that is, water not saturated with respect to calcium, gradually dissolves the calcium in the cement-based grout fillings of ceramic-tiled pools. In an example scenario, in a pool operated with unbalanced water chemistry the emptying out of the grout joints within a few years can lead to water leaks and surfaces that harbour algae. PVC-based liner coverings, by contrast, are synthetic polymers that contain no calcium binder in their structure; for this reason they are not affected by the water's tendency to dissolve calcium through the same mechanism. This does not mean that a liner covering can go without maintenance under all conditions: water chemistry balance must be maintained in every case for the sake of the equipment and hygiene.

Choosing a pool surface without knowing the chemistry of the water means making an investment without doing the arithmetic. While soft, unbalanced water leads to dissolution in cement-based grout joints, this calcium dissolution mechanism does not arise on a polymer liner surface.

01. The Effect of Low Calcium Hardness and Unbalanced Water on Cement Grout Joints

The chemical erosion process that can be seen in ceramic-tiled pools filled with soft mains water and operated without balancing is as follows:

  • Calcium Undersaturation: The calcium hardness range in which pool water is considered balanced is typically given as between 200 and 400 ppm. If the measured value is appreciably below this range (as a planning assumption, for example between 60 and 80 ppm), the water tends to dissolve the free lime and calcium hydroxide in the grout filling.
  • Emptying of Grout Joints and Falling Tiles: Grout whose binder has dissolved can turn powdery. If water seeps through the resulting voids, the adhesive layer behind may be damaged and the covering elements may begin to detach.
  • The Effect of Acid Rain: Slightly acidic rainwater mixing into the pool can lower the pH value and increase the water's corrosive tendency. The magnitude of this effect depends on the rainfall regime, whether or not the pool is open to the sky, and the water balance.
  • The Periodic Grout Renewal Cycle: In pools that suffer grout loss, a need for grout renewal may arise at certain intervals; this both creates a labour cost and the fine material released can contaminate the filter sand. The frequency of renewal varies with water chemistry and workmanship quality, so no fixed schedule can be given.

02. Langelier Saturation Index (LSI) Balance and the Chemical Behaviour of Liner Coverings

The LSI index is used to assess whether water has a corrosive tendency or a scale-forming one (LSI = pH + TF + CF + AF - 12.1):

  1. Negative LSI Condition: When the LSI value falls below roughly -0.3, the water shows a corrosive tendency. For example, water measured between -0.5 and -0.8 carries the risk of dissolving cement-based surfaces and corroding metals. These values are hypothetical examples; measurement is required for every pool.
  2. The Liner Membrane Contains No Minerals: PVC-based liner covering contains no calcium or lime-based binder within its body. For this reason, even if the water is not saturated with respect to calcium, no calcium dissolution takes place from the liner surface. The liner can nonetheless be affected by UV, extreme pH deviations and intensive chemical contact; describing it as entirely unaffected chemically would not be accurate.
  3. Reduced Need to Raise Hardness: In ceramic-tiled pools, the water is balanced with calcium hardness increasing products in order to protect the grout joints. In a liner-covered pool there are no cement-based grout joints, so hardness adjustment is made primarily to protect the equipment; the quantity of product used is calculated according to the pool volume and the measured values.
  4. Contact with a Smooth Surface: A joint-free, smooth surface reduces the risk of scratches caused by a tile coming loose or a grout edge becoming sharp.

03. Water Chemistry Comparison Table: Pool with Cement Grout Joints versus Liner-Covered Pool

Chemical ParameterCement-Grouted Ceramic / MosaicSermed Antibacterial Liner Membrane
Response to Calcium UndersaturationIn unbalanced water, dissolution and emptying of the grout joints can be seenDoes not erode by this mechanism because it contains no calcium binder
Compatibility with Soft WaterPoor (the hardness balance of the water has to be established)Good (no calcium dissolution problem arises in soft water)
pH FluctuationWhen the lime in the grout dissolves, the pH and hardness values of the water can changeNo mineral is contributed from the surface; pH balance depends on chemical management
Algae HarbouringEmptied grout gaps create a footing for algae to take holdAlgae find it harder to take hold on a smooth surface, though maintenance is still required
Periodic Grout CostAs grout is lost, a budget for grout filling is neededSince there are no grout joints, no grout filling cost arises

Conclusion: Operating a ceramic-grouted pool with soft, unbalanced water calls for regular grout maintenance. Liner covering removes the problem of grout-related calcium dissolution through the choice of material; water chemistry management, however, continues in both systems.

Frequently asked questions

Why do ceramic grout joints erode in soft mains water, and why does this mechanism not occur with a liner covering?

Water with low calcium hardness tends to dissolve the free calcium in cement-based grout joints in order to reach its chemical balance, and over time this can lead to grout loss. Because PVC-based liner membranes have a synthetic polymer structure containing no calcium binder, they do not erode through this dissolution mechanism. The rate of erosion depends on the measured values of the water and on maintenance discipline.

Does low-calcium water damage pool equipment?

Unbalanced water with a corrosive tendency can accelerate corrosion in metal components such as chlorine generator plates and heat pump heat exchangers. For this reason it is recommended that the LSI balance of the water be kept roughly between -0.3 and +0.3; target values should be verified against the equipment manufacturer's instructions.

What should the calcium hardness be, in ppm, in liner pools?

While higher hardness ranges are generally recommended in ceramic pools in order to protect the grout joints, in liner pools hardness adjustment is mainly aimed at protecting the equipment. Example planning ranges can be given as 250 to 350 ppm for ceramic and 150 to 200 ppm for liner; the binding reference is the equipment used, the label information of the chemical products and the measured water analysis.

Can a liner covering be applied over grout joints that have emptied out?

In most cases it is possible. Felt can be laid inside an old ceramic pool with eroded grout joints and a 1.50 mm reinforced liner applied to obtain a joint-free water surface. Suitability depends on an engineer's assessment of factors such as the structural condition of the existing shell, the cause of the leak and the groundwater level.

Frequently asked questions →
Sermed Havuz technical team

Source: Sermed Havuz technical materials

Request a consultation →

Your next summer starts here.

Share your location and a photo of your space. We’ll help you choose a pool and cover.